Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 126 °C
259 °F
ISO 75-1/-2
Lanxess Pocan® B 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant
Deflection Temperature at 8.0 MPa 126 °C
259 °F
ISO 75-1/-2
Lanxess Pocan® BF 4225 000000 PBT, 20% Glass Fiber
PBT, 20% glass fibers, injection molding, flame retardant