Glow Wire Test 950 °C

@Thickness 3.00 mm
1740 °F

@Thickness 0.118 in
GWFI; IEC 60695-2-12
PTS PCA-2201NH Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 950 °C

@Thickness 3.00 mm
1740 °F

@Thickness 0.118 in
GWFI; IEC 60695-2-12
PTS PCA-2201NHV Non Bromine, Non Chlorine Flame Retardant Polycarbonate/ABS Alloy, UV Stabilized
Information provided by Polymer Technology and Services, LLC (PTS).
Glow Wire Test 950 °C

@Thickness 0.750 mm
1740 °F

@Thickness 0.0295 in
IEC 60695-2-12
DuPont Performance Polymers Rynite® GW520CS NC010 PET  (Unverified Data**)
Rynite® GW520CS NC010 is a 20% glass fiber reinforced, flame retardant, color stabilized, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
(GWFI); IEC 60695-2-12
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
(GWIT); IEC 60695-2-13
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures ..
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
(GWFI); IEC 60695-2-12
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
(GWIT); IEC 60695-2-13
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
Index; IEC 60695-2-12
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi..
Glow Wire Test 950 °C

@Thickness 2.00 mm
1740 °F

@Thickness 0.0787 in
GWFI; IEC 60695
Eurotec® Tecolen® HP30 NL XC30 PPHP, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Glow Wire Test 950 °C

@Thickness 3.00 mm
1740 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
Ascend Performance Materials Vydyne® 66J Nylon 66, General Purpose, high viscosity, DAM
Vydyne® 66J is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66J resin offers high strength, ..