Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips 1008.5 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 112, A 14200Characteristics: Excellent Flexibility, Excellent Flow, Good Warping Resistance, Moderate Mold Release, Moderate ESCRApplications:.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips 1400 Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Good Flexibility, Good Flow, Good Warping Resistance, Good Mold Release, Good ESCRApplications:Lids & Closures, C.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips 4538B LDPE Injection Molding Resin
(discontinued **) Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 05200Characteristics: Good Flexibility, Moderate Flow, Moderate Warping Resistance, Good Mold Release, Excellent ESCRApplications:Perso.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
ExxonMobil Escorene® LD-400 LDPE Medium/High Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer resin designed for electrical applications.Applications: Base resin for medium voltage power cable insulati.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
ExxonMobil Escorene® LD-411 LDPE Power Cable Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable polyethylene homopolymer designed as an electrical grade base resin especially suitable for Henschel blending.Applications: A base r.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
ExxonMobil Escorene® LD-401 EVA for Electrical Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Base resin for fully formulated low voltage cable i.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips Marlex® 1007 Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 25200Characteristics: Excellent Flexibility, Good Flow, Good Warping Resistance, Moderate Mold Release, Good ESCRApplications:Houseware.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips Marlex® 1122B Injection Molding Resin Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati.. |
|||
Brittleness Temperature | <= -72.0 °C | <= -97.6 °F | ASTM D746 |
Chevron Phillips Marlex® 5104 LDPE Blow Molding Resin Resin Type: HomopolymerCharacteristics: High Melt Strength, Good Parison Control, Good Stability, Low Taste and Odor Characteristics, Good Impact and Toughness, Good Clarity on Gloss, Long Standing .. |
|||
Brittleness Temperature | -72.0 °C | -97.6 °F | ASTM D746 |
Colorite Polymers 8080 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -72.0 - -3.00 °C | -97.6 - 26.6 °F | Average value: -36.8 °C Grade Count:179 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |