Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -72.0 - -3.00 °C | -97.6 - 26.6 °F | Average value: -36.8 °C Grade Count:179 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |