Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
LG Chemical KEYFLEX TO-1075A Thermoplastic Olefin for Injection Molding, 75A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
Kraton® G7705 GI-B (SEBS) Compound Description: Kraton G7705 GI-B is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
Kraton® G7705 GI-N (SEBS) Compound Description: Kraton G7705 GI-N is an easy processing, general purpose 44 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D 746 |
Zylog Neoplast® 135 FT EB Thermoplastic Vulcanizate Neoplast 135 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, .. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | XT<sub>b</sub>; ASTM D746 |
Colorite Polymers Elastichem 3511TX-02 Vinyl Compound Description: All components in Elastichem are sanctioned by the U.S. Food & Drug Administration for food packaging applications under Title 21 of the Code of Federal Regulations. For medical use, co.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
Colorite Polymers 3511-02 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
Colorite Polymers 6588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedNaturalApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionConsumer GoodsIndustrialProcessing Method:Injecti.. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D-746 |
Axiall 491 Wire & Cable Flexible PVC 60°C rated low temperature jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -63.0 °C | -81.4 °F | ASTM D746 |
Kraton® G7720 GI-N (SEBS) Compound Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |