Axiall 491 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 491 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60°C rated low temperature jacketing compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.24 - 1.28 g/cc
1.24 - 1.28 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 79
73 - 79
delayed; ASTM D-2240
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D-638
Elongation at Yield 261.8 %
261.8 %
Oil Aging: 4 hours @ 70°C; #2 Oil; 30 mil slabs; UL 1581
279 %
279 %
Air Aging: 7 days @ 100°C; 30 mil slabs; UL 1581
350 %
350 %
ASTM D-638
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -63.0 °C
-81.4 °F
ASTM D-746
Oxygen Index 25 %
25 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 174 °C
345 °F