Material Notes:
Neoplast 135 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 38
38
ASTM D 2240
40

@Time 605000 sec
40

@Time 168 hour
Heat Aging; ASTM D 2240/ASTM D 573
Tensile Strength, Ultimate 2.65 MPa
384 psi
500 mm/min; ASTM D 412
1.96 MPa

@Time 605000 sec
284 psi

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 300 %
300 %
500 mm/min; ASTM D 412
240 %

@Time 605000 sec
240 %

@Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.00147 GPa
0.213 ksi
500 mm/min; ASTM D 412
Tear Strength 9.81 kN/m
56.0 pli
500 mm/min; ASTM D 624
Compression Set 14 %

@Temperature 23.0 °C,
Time 79200 sec
14 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Brittleness Temperature -63.0 °C
-81.4 °F
ASTM D 746