Material Notes:
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Instant; ASTM D2240
Tensile Strength, Yield 4.07 MPa
590 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
2.45 MPa

@Strain 300 %
355 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 580 %
580 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 43 %
43 %
Bayshore; ASTM D2632
Tear Strength 22.1 kN/m
126 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 13 %
13 %
Method B, 73°F(23°C), 22 hrs; ASTM D395
Thermal Properties Metric English Comments
Brittleness Temperature -56.0 °C
-68.8 °F
ASTM D746
Flammability, UL94 V-0
V-0
Natural, 0.062 in thick; UL 94
Oxygen Index 27 %
27 %
0.062 in. bars; ASTM D2863