Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Brittleness Temperature = -51.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing
Tygon S3â„¢ E-3603 from Saint-Gobain Performance Plastics is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable, flexible tubing products. The bio-ba..
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation
Tygon S3â„¢ E-LFL from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-base..
Brittleness Temperature -46.1 °C
-51.0 °F
ASTM D746
Teknor Apex APEX® 3211-50 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling..