Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -46.1 °C | -51.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B65B1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -46.1 °C | -51.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible C70T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -46.1 °C | -51.0 °F | ASTM D746 |
Saint-Gobain Tygon® S3™ E-3603 Phthalate-free Vacuum and Laboratory Tubing Tygon S3™ E-3603 from Saint-Gobain Performance Plastics is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable, flexible tubing products. The bio-ba.. |
|||
Brittleness Temperature | -46.1 °C | -51.0 °F | ASTM D746 |
Saint-Gobain Tygon® S3™ E-LFL Long-Flex Life Pump Tubing Formulation Tygon S3™ E-LFL from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-base.. |
|||
Brittleness Temperature | -46.1 °C | -51.0 °F | ASTM D746 |
Teknor Apex APEX® 3211-50 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |