Polymer Property : Brittleness Temperature = -30.5 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Brittleness Temperature -30.5 °C
-22.9 °F
The Chemical Company ChemFlexx™ 206 Phthalate Plasticizer
Chemflexx 206 is considered to be a “functional replacement” for linear plasticizers. It is an organic, non-hazardous, liquid, phthalate ester. Chemflexx 206 is a plasticizer for the manufacture ..