The Chemical Company ChemFlexx™ 206 Phthalate Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer The Chemical Company
Trade Name ChemFlexx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF The Chemical Company ChemFlexx™ 206 Phthalate Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemflexx 206 is considered to be a “functional replacement” for linear plasticizers. It is an organic, non-hazardous, liquid, phthalate ester. Chemflexx 206 is a plasticizer for the manufacture of flexible plastics. End use applications include PVC floor coverings, roofing membranes, swimming pool liners and wall coverings, expanded leather, PVC foams, films, sealing and adhesive systems based on poly urethane or polysulphide, soft squeeze toys, balls, vinyl upholstery, tablecloths, shower curtains, raincoats, and a range of other products that must stay flexible for the lifetime of their use.Information provided by The Chemical Company
Physical Properties Metric English Comments
Specific Gravity 0.966 - 0.977 g/cc

@Temperature 20.0 °C
0.966 - 0.977 g/cc

@Temperature 68.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 81
81
15 sec. delay
87
87
Instant
Tensile Strength, Ultimate 16.487 MPa
2391.2 psi
oven aged 7 days @ 113°C
16.8 MPa
2440 psi
16.8 MPa
2440 psi
oven aged 10 days @ 100°C
Elongation at Break 329 %
329 %
oven aged 7 days @ 113°C
354 %
354 %
354 %
354 %
oven aged 10 days @ 100°C
100% Modulus 0.01351 GPa
1.959 ksi
Thermal Properties Metric English Comments
Brittleness Temperature -30.5 °C
-22.9 °F
Oxygen Index 30 %
30 %
Chemical Properties Metric English Comments
Acid Value <= 0.010
<= 0.010
parent acid %
<= 0.070
<= 0.070
mg KOH/g
Descriptive Properties Value Comments
Alcohol Content = 1000ppm
Appearance Clear and free of suspended matter
Assay = 99.6%
Hazen Color Value (pt-co) = 35
Weight Loss (%) 1
oven aged 10 days @ 100°C
4
oven aged 7 days @ 113°C