Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -30.5 °C | -22.9 °F | |
The Chemical Company ChemFlexx™ 206 Phthalate Plasticizer Chemflexx 206 is considered to be a “functional replacement” for linear plasticizers. It is an organic, non-hazardous, liquid, phthalate ester. Chemflexx 206 is a plasticizer for the manufacture .. |