Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -3.00 °C | 26.6 °F | ASTM D746 |
Colorite Polymers CS7566LS Wire and Cable Jacket Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -3.00 °C | 26.6 °F | |
AlphaGary PVC GM 8017 Natural Polyvinyl Chloride Thermoplastic A lead and cadmium free, flame retardant, 105°C, UL-94 V-O or V-2 rated, non-migrating, electrical grade, semi-rigid molding compound |
|||
Brittleness Temperature | -3.00 °C | 26.6 °F | |
AlphaGary Smokeguard™ LS III 1093 Low Smoke Polyvinyl Chloride 75°C Plenum Jacket |
|||
Brittleness Temperature | -3.00 °C | 26.6 °F | ASTM D-746 |
Axiall 01590 Plenum Flexible PVC Non-lead stabilized plenum grade insulation compound for Category 3 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -3.00 °C | 26.6 °F | ASTM D-746 |
Axiall H 3182A Plenum Flexible PVC Plenum-grade insulation compound for Category 3 applications. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -3.00 °C | 26.6 °F | |
AlphaGary Smokeguard™ LS III 1091 A1 Low Smoke Polyvinyl Chloride 60°C Plenum Jacket |