AlphaGary PVC GM 8017 Natural Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer AlphaGary
Trade Name PVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC GM 8017 Natural Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A lead and cadmium free, flame retardant, 105°C, UL-94 V-O or V-2 rated, non-migrating, electrical grade, semi-rigid molding compound
Mechanical Properties Metric English Comments
Hardness, Shore D 38 - 55
38 - 55
Tensile Strength 13.1 MPa
1900 psi
Elongation at Break 150 %
150 %
ASTM D412
Thermal Properties Metric English Comments
Brittleness Temperature -3.00 °C
26.6 °F
Flammability, UL94 V-2
V-2
V-0
V-0
Oxygen Index 28 %
28 %