Axiall H 3182A Plenum Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall H 3182A Plenum Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plenum-grade insulation compound for Category 3 applications. UL QMTM2 plenum cable compound component.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.48 - 1.52 g/cc
1.48 - 1.52 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 60 - 66
60 - 66
delayed; ASTM D-2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 270.6 %
270.6 %
Air Aging: 7 days @ 100°C; 75-mil plaques; UL 1581
291 %
291 %
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -3.00 °C
26.6 °F
ASTM D-746
Oxygen Index 38 %
38 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 3.18

@Frequency 1e+6 Hz
3.18

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F
Users viewing this material also viewed the following: