Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable JJF102L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable MJF114A Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
S&E Specialty Polymers TufFlex™ GA-1042FR-60-0-405 Black TPE Compound Application: An oil resistant, flexible, 60°C rated jacketing compound.Information provided by S&E Specialty Polymers |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3887 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3901 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible 86155 Polyvinyl Chloride, Flexible (PVC, Flexible) 86155 is a flexible (90A durometer) vinyl compound formulated from FDA-santioned raw materials. This compound has received NSF Standard 61 only for sheets applications.NOTE: All ingredients used in .. |
|||
Brittleness Temperature | <= -27.0 °C | <= -16.6 °F | F<SUB>50</SUB>; ASTM D746 |
LyondellBasell Petrothene® GA594189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA594189 is a pelletized LLDPE copolymer resin for injection molding thin-walled items requiring high flow and short cycle times. GA594189 exhibits excellent flow, warp resistance and sur.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 3200-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 3611-85 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 4130 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Good UV Resistance; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing Forms: Pellets Agency Ratings: UL QMTT2 .E73402 Wire Types: SJTW; STW.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 468 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Oil Resistant Uses: Armored Cable; Military Cable Jacketing Forms: Pellets Processing Method: Extrusion Agency Ratings: MIL C-2194-D.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 65004 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Communication Wire JacketingForms: Pellets Agency Ratings: NEC Article 725; NEC Article 760; NEC.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 65007 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
Teknor Apex APEX® 97-G0029C-82 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS CompliantFeatures: Flame Retardant Uses: Cable Jacketing; Communication Wire JacketingAgency Ratings: UL 62; UL 444 Forms: Pellets Processing Method: ExtrusionInformation.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Sylvin Technologies 500 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Sylvin Technologies 6137-85 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Colorite Polymers 8311 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Colorite Polymers 8312 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Colorite Polymers Self Frosting™ 8311SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PHA 78 Flexible PVC, Transparent Extrusion Atoxic pipes |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Aearo E-A-R Specialty Composites Isoloss® HD Polyurethane Elastomer Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protect.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D-746 |
Axiall 38900 Wire & Cable Flexible PVC Low cost AWM jacket for SPT, SVT, SJT applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
Aearo E-A-R Specialty Composites Isoloss® HDF Polyurethane Elastomer Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protect.. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | |
AlphaGary PVC FMPP - Clear, Various Colors Polyvinyl Chloride Thermoplastic Resistant to UV, moisture and mildew for high speed extrusion of coated yarn for outdoors furniture, wire fence coating and automotive harness cable coating |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 5 Flexible PVC, Extrusion Tunnel waterproofing |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 67/FR Flexible PVC, Lead Free Spiral pipes, UL 94 Class V0 |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 7005 Flexible PVC, Lead Free Pipes and profiles |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D-746 |
Axiall 50898 Moldings & Extrusions Flexible PVC Migration resistant, flexible PVC compound recommended for injection molding and extrusion applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable 1721-xx14E Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -27.0 °C | -16.6 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 80/R1 Flexible PVC, Lead Free Water pipes |