AlphaGary PVC FMPP - Clear, Various Colors Polyvinyl Chloride Thermoplastic

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Extruded , PVC, Wire and Cable Grade
Manufacturer AlphaGary
Trade Name PVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary PVC FMPP - Clear, Various Colors Polyvinyl Chloride Thermoplastic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resistant to UV, moisture and mildew for high speed extrusion of coated yarn for outdoors furniture, wire fence coating and automotive harness cable coating
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Tensile Strength 17.9 MPa
2600 psi
Thermal Properties Metric English Comments
Brittleness Temperature -27.0 °C
-16.6 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified