Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -103 °C | <= -153 °F | ASTM D746 |
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed.. |
|||
Brittleness Temperature | <= -103 °C | <= -153 °F | ASTM D746 |
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |