Thermal Properties Metric English Comments
Brittleness Temperature <= -103 °C
<= -153 °F
ASTM D746
ExxonMobil EXACT™ 8230 Plastomer for Polymer Modification
Product Description: Exact 8230 plastomer is an ethylene octene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties. It is designed..
Brittleness Temperature <= -103 °C
<= -153 °F
ASTM D746
Chevron Phillips HiD® 9512/HiD® 9513 with Antistat HDPE Blow Molding Resin  (discontinued **)
Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo..