Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -112 °C | -170 °F | ASTM D746 |
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Brittleness Temperature | -112 °C | -170 °F | ASTM D746 |
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit.. |
|||
Brittleness Temperature | -112 - -71.0 °C | -170 - -95.8 °F | Average value: -98.0 °C Grade Count:12 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |