Thermal Properties Metric English Comments
Brittleness Temperature -112 - -71.0 °C
-170 - -95.8 °F
Average value: -98.0 °C Grade Count:12
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..