Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 650 - 700 °C | 1200 - 1290 °F | Average value: 662 °C Grade Count:30 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |