Polymer Property : Glow Wire Test = 1290 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glow Wire Test 650 - 700 °C
1200 - 1290 °F
Average value: 662 °C Grade Count:30
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..