Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 75.0 - 110 °C | 167 - 230 °F | Average value: 87.2 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
UL RTI, Mechanical without Impact | 50.0 - 110 °C | 122 - 230 °F | Average value: 90.0 °C Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |