Polymer Property : UL RTI, Mechanical with Impact = 176 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 65.0 - 80.0 °C
149 - 176 °F
Average value: 72.5 °C Grade Count:3
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
UL RTI, Mechanical with Impact 60.0 - 80.0 °C
140 - 176 °F
Average value: 63.3 °C Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..