Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 - 80.0 °C | 165 - 176 °F | with 160°C Thermal Postcure; ASTM D648 |
Proto3000 Accura® 50 Plastic Stereolithography (SLA) Prototyping Polymer Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 80.0 °C | 167 - 176 °F | after thermal post treatment procedure A; ASTM D648-06 |
Proto3000 Objet RGD525 High Temperature Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.0 - 80.0 °C | 165 - 176 °F | with 160ºC thermal postcure; ASTM D648 |
3D Systems Accura® 50 Plastic for SLA® Systems Simulate the properties and appearance of molded ABS. For use with the Viper™ SLA® system, SLA 3500, SLA 5000 and SLA 7000 systems.ApplicationsFunctional components for assemblies, mock-ups and te.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 80.0 °C | 167 - 176 °F | |
C.O.I.M. EXTER S® S 111 B Orthophthalic Resin Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 111 B: Low viscosity.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 34.0 - 80.0 °C | 93.2 - 176 °F | Average value: 45.3 °C Grade Count:24 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |