Material Notes:
Simulate the properties and appearance of molded ABS with this durable, accurate and versatile plastic.Features:Durable and stiffOutstanding accuracy w/out shrinkage related distortionChoice of grey or natural colorsFully developed and tested build stylesBenefits:Produce ABS like parts without machining or moldingColor selection produces parts that have the appearance of molded plasticRigidity holds shape on thin walls, but flexes for snap fit assembliesProduces parts that meet tolerancesProduces parts that are faithful to the CADMaximize reliability with no user R&DApplications:Functional components for assemblies, mock-ups and test for many uses, including:- Enclosures, covers and cases for consumer goods- Toys- Cellular/mobile telephones- Electronic components: connectors, interconnects, routing enclosures, etc.- Automotive design elements: dash boards, air conditioning vents, etc.Accurate, durable master patterns for RTV or silicone moldingLimited snap-fits and assembliesSimulate a molded partConcept modelsMarketing modelsInformation provided by Proto3000 for their protoyping engineering services.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
Liquid
1.21 g/cc
0.0437 lb/in³
Solid
Viscosity 600 cP

@Temperature 30.0 °C
600 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength at Break 48.0 - 50.0 MPa
6960 - 7250 psi
ASTM D638
Elongation at Break 5.3 - 15 %
5.3 - 15 %
ASTM D638
Tensile Modulus 2.48 - 2.69 GPa
360 - 390 ksi
ASTM D638
Flexural Strength 72.0 - 77.0 MPa
10400 - 11200 psi
ASTM D790
Flexural Modulus 2.21 - 2.34 GPa
321 - 339 ksi
ASTM D790
Izod Impact, Notched 0.165 - 0.281 J/cm
0.309 - 0.526 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 0.730 µm/m-°C

@Temperature 0.000 - 20.0 °C
0.406 µin/in-°F

@Temperature 32.0 - 68.0 °F
T<Tg; ASTM E831-93
1.64 µm/m-°C

@Temperature 90.0 - 150 °C
0.911 µin/in-°F

@Temperature 194 - 302 °F
T>Tg; ASTM E831-93
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 53.0 °C
120 - 127 °F
ASTM D648
74.0 - 80.0 °C
165 - 176 °F
with 160°C Thermal Postcure; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.0 - 46.0 °C
109 - 115 °F
ASTM D648
Glass Transition Temp, Tg 62.0 °C
144 °F
DMA, E"
Descriptive Properties Value Comments
Appearance Opaque natural or opaque grey
Critical Exposure (Ec) 9.0 mJ/cm2
Penetration Depth (Dp) 4.5 mils