Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 34.0 °C | 93.2 °F | ASTM D648 |
DuPont™ Surlyn® 8670 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8670 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 34.0 - 80.0 °C | 93.2 - 176 °F | Average value: 45.3 °C Grade Count:24 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |