Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 267 - 284 °C | 513 - 543 °F | with 120°C Thermal Postcure; ASTM D648 |
Proto3000 Accura® Bluestone™ Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features:Exceptional stiffnessHigh temperature resistanceExcellent accuracyHigh humidi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 267 °C | 513 °F | HDT B; Unannealed; ISO 75-2/B |
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 267 °C | 513 °F | HDT B; Unannealed; ISO 75-2/B |
Solvay Specialty Polymers Lavanta® 5115 WH 251 Polyester, High Performance (HPP), 15% Glass Fiber Lavanta® 5115 WH 251 is a high-performance polyester (HPP) is a 15% glass reinforced, injection molding grade developed specifically for HB LED packaging applications that utilize surface mount t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 267 °C @Thickness 6.40 mm |
513 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific) PPE+PPS GF30% |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 267 - 284 °C | 513 - 543 °F | with 160ºC thermal postcure; ASTM D648 |
3D Systems Accura® Bluestone™ Plastic for SLA® Systems A high stiffness engineered nanocomposite that opens new applications for stereolithography users. For use with solid-state stereolithography (SLA®) systems.ApplicationsWind-tunnel testing for the .. |