Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name NORYL GTX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PPS GF30%
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0025 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 29.1 g/10 min

@Load 5.00 kg,
Temperature 300 °C
29.1 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 112 MPa
16200 psi
SABIC - Japan Method
Elongation at Break 8.0 %
8.0 %
SABIC - Japan Method
Flexural Strength 156 MPa
22600 psi
ASTM D790
Flexural Modulus 8.43 GPa
1220 ksi
ASTM D790
Izod Impact, Notched 0.880 J/cm
1.65 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 25.0 - 55.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
13.9 - 30.6 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 267 °C

@Thickness 6.40 mm
513 °F

@Thickness 0.252 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Dielectric Constant 3.3

@Frequency 50.0 - 60.0 Hz
3.3

@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 22.1 kV/mm

@Thickness 1.60 mm
561 kV/in

@Thickness 0.0630 in
in oil; ASTM D149