Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA
LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant.
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
HDT B; Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
HDT B; Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry)
Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f..
Deflection Temperature at 0.46 MPa (66 psi) >= 298 °C

@Thickness 3.20 mm
>= 568 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LC006 PEEK
LNP THERMOCOMP* LC006 is a compound based on Polyetheretherketone resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Deflection Temperature at 0.46 MPa (66 psi) >= 298 °C

@Thickness 3.20 mm
>= 568 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK
LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) >= 298 °C

@Thickness 3.20 mm
>= 568 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific)
LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Deflection Temperature at 0.46 MPa (66 psi) >= 298 °C

@Thickness 3.20 mm
>= 568 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Deflection Temperature at 0.46 MPa (66 psi) 298 °C
568 °F
Unannealed; ISO 75-2/B
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom..