Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
Nilit Polynil® P200 High Viscosity Nylon 66 Description: High viscosityApplication: Semi-finished and FilmInformation provided by NILIT. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-GP1 General Purpose Nylon 66 General Purpose Nylon 66, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | ASTM D648 |
Polymer Resources NY66-GP1-[color]H Nylon, General Purpose Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 445 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP Thermocomp RW008XXZ PA 66 LNP* Thermocomp* RW008XXZ is a compound based on Nylon 6/6 resin containing Wollastonite.This data was supplied by SABIC-IP for the Americas region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® NN100TL (Dry) Nylon 66, Lubricated, Impact Modified Features: LubricatedImpact modifiedGood toughnessForm: PelletsInformation provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
Adell AT-13 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
A. Schulman ComAlloy Comtuf® 633 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
Ashley Polymers Ashlene® 559LD-33G Nylon 66, 33% Glass Reinforced A high impact reinforced nylon copolymer with good low temperature properties.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 229 °C | 444 °F | ASTM D648 |
Adell AT-33 Nylon 66, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |