A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass Reinforced, Impact Grade
Manufacturer A. Schulman ComAlloy
Trade Name COMTUF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comtuf® 630 Nylon 6/6, Glass Reinforced, Impact Modified, Flow Enhanced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 121 MPa
17500 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 7.60 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 255 - 275 °C
491 - 527 °F
Deflection Temperature at 0.46 MPa (66 psi) 229 °C
444 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
406 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
Approximate middle barrel temperature.