Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 - 98.0 °C
172 - 208 °F
Average value: 87.8 °C Grade Count:12
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..