Material Notes:
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent surface finishGood thermal performanceInformation provided by NILIT.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792, ISO 1183
Water Absorption 0.20 %
0.20 %
23°C, 24h in H<sub>2</sub>O; sim. ISO 62
Water Absorption at Saturation 0.50 %
0.50 %
sim. ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
Euronil
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
Euronil
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
ISO 527, ASTM D638
Elongation at Break 35 %
35 %
ISO 527, ASTM D638
Elongation at Yield 4.0 %
4.0 %
ISO 527, ASTM D638
Flexural Yield Strength 85.0 MPa
12300 psi
ISO 178, ASTM D790
25.0 MPa

@Temperature 90.0 °C
3630 psi

@Temperature 194 °F
ISO 178, ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ISO 178, ASTM D790
0.500 GPa

@Temperature 90.0 °C
72.5 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched >= 25.0 J/cm²
>= 119 ft-lb/in²
ISO 179
>= 4.00 J/cm²

@Temperature -30.0 °C
>= 19.0 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179
0.400 J/cm²

@Temperature -30.0 °C
1.90 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75, ASTM D648
Vicat Softening Point 191 °C
376 °F
49 N; ISO 306, ASTM D1525
205 °C
401 °F
9.8 N; ISO 306, ASTM D1525
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Oxygen Index 22 %
22 %
ASTM D2863
Glow Wire Test 850 °C

@Thickness 3.20 mm
1560 °F

@Thickness 0.126 in
Glow Wire Flammability Index; IEC 694-2-12
850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
Glow Wire Flammability Index; IEC 694-2-12
Electrical Properties Metric English Comments
Dielectric Strength 19.0 kV/mm

@Thickness 2.00 mm
483 kV/in

@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index 350 V

@Thickness 3.20 mm
350 V

@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
600 V

@Thickness 3.20 mm
600 V

@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
Descriptive Properties Value Comments
Heat Resistance - Ball Test OK
at 125°C, IEC 309
OK
at 165°C, IEC 309