Material Notes:
Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with no mechanical load. Murflor® also has the lowest dynamic friction coefficient of all thermoplastics.Special Properties:• Best dynamic friction properties of all thermoplastics• No stick/slip effect• Very good anti-adhesion properties• Electrically isolating• Very high resistance to chemicals• Very high resistance to hydrolysis• Very tough, even at low temperatures• Approved for use in the food industry (FDAInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 2.18 g/cc
0.0788 lb/in³
ISO 1183-1
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
DIN 53505
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527-1/-2
Elongation at Break 300 %
300 %
ISO 527-1/-2
Modulus of Elasticity 0.750 GPa
109 ksi
Compressive Yield Strength 4.50 MPa

@Strain 1.00 %
653 psi

@Strain 1.00 %
dry; ISO 604
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.080
0.080
Sand Slurry 21
21
µm/km
Thermal Properties Metric English Comments
CTE, linear 160 µm/m-°C

@Temperature 23.0 - 100 °C
88.9 µin/in-°F

@Temperature 73.4 - 212 °F
Melting Point 321 °C
610 °F
ISO 11357-1
Maximum Service Temperature, Air 260 °C

@Time 7.20e+7 sec
500 °F

@Time 20000 hour
300 °C

@Time <=86400 sec
572 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -200 °C
-328 °F
Glass Transition Temp, Tg 127 °C
261 °F
ISO 11357-1
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Dielectric Constant 2.0

@Frequency 100 Hz
2.0

@Frequency 100 Hz
IEC 60250
2.1

@Frequency 1.00e+6 Hz
2.1

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 20.0 kV/mm
508 kV/in
IEC 60243-1
Dielectric Loss Index 0.00010

@Frequency 1.00e+6 Hz
0.00010

@Frequency 1.00e+6 Hz
IEC 60250
0.00030

@Frequency 100 Hz
0.00030

@Frequency 100 Hz
IEC 60250
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Natural
Users viewing this material also viewed the following: