Thermal Properties Metric English Comments
CTE, linear 139 µm/m-°C

@Temperature 100 - 200 °C
77.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler  (discontinued **)
Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div..
CTE, linear 139 µm/m-°C

@Temperature 100 - 200 °C
77.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.