Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 139 µm/m-°C @Temperature 100 - 200 °C |
77.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
CTE, linear | 139 µm/m-°C @Temperature 100 - 200 °C |
77.0 µin/in-°F @Temperature 212 - 392 °F |
ASTM E831 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |