Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 - 7.90 µm/m-°C @Temperature 25.0 - 100 °C |
3.61 - 4.39 µin/in-°F @Temperature 77.0 - 212 °F |
|
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |