Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 6.50 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.50 µm/m-°C

@Temperature 300 °C
3.61 µin/in-°F

@Temperature 572 °F
MarkeTech Repton 115 Aluminum Oxide
Brand 115 features: High Density and Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even whe..
CTE, linear 6.50 µm/m-°C

@Temperature 300 °C
3.61 µin/in-°F

@Temperature 572 °F
MarkeTech Repton 125 Aluminum Oxide
Brand 125 features: High Purity Standard.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t..
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 °C
3.61 µin/in-°F

@Temperature 68.0 °F
c direction
Momentive Performance Materials "PG" Pyrolytic Graphite
Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne..
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 300 °C
3.61 µin/in-°F

@Temperature 68.0 - 572 °F
H.C. Starck HPM 1710 Tungsten High Density Composite
Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe..
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 450 °C
3.61 µin/in-°F

@Temperature 68.0 - 842 °F
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t..
CTE, linear 6.50 - 7.90 µm/m-°C

@Temperature 25.0 - 100 °C
3.61 - 4.39 µin/in-°F

@Temperature 77.0 - 212 °F
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO
Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop..
CTE, linear 6.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.61 µin/in-°F

@Temperature -22.0 - 158 °F
Schott K10 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.61 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-BALF4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.61 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK11 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.61 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SK4 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 300 °C
3.61 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-SK5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 6.50 µm/m-°C

@Temperature -30.0 - 70.0 °C
3.61 µin/in-°F

@Temperature -22.0 - 158 °F
Schott NG3 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 400 °C
3.61 µin/in-°F

@Temperature 68.0 - 752 °F
CeramTec Rubalit® A 1894 Alumina, 94%
Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond ..
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 200 °C
3.61 µin/in-°F

@Temperature 68.0 - 392 °F
DIN EN 821-1
CeramTec Rubalit® IS 95 Alumina
Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva..
CTE, linear 6.50 µm/m-°C

@Temperature 20.0 - 200 °C
3.61 µin/in-°F

@Temperature 68.0 - 392 °F
hardened to 62 HRC
Bohler-Uddeholm O1 Cold Work Tool Steel
Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha..
Copyright © lookpolymers.com All Rights Reserved