Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 6.50 µm/m-°C @Temperature 300 °C |
3.61 µin/in-°F @Temperature 572 °F |
|
MarkeTech Repton 115 Aluminum Oxide Brand 115 features: High Density and Purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even whe.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 300 °C |
3.61 µin/in-°F @Temperature 572 °F |
|
MarkeTech Repton 125 Aluminum Oxide Brand 125 features: High Purity Standard.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when t.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 °C |
3.61 µin/in-°F @Temperature 68.0 °F |
c direction |
Momentive Performance Materials "PG" Pyrolytic Graphite Pyrolytic Graphite (PG) is a unique form of graphite manufactured by decomposition of a hydrocarbon gas at very high temperature in a vacuum furnace. The result is an ultra-pure product which is ne.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 300 °C |
3.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck HPM 1710 Tungsten High Density Composite Description of Product: Tungsten based composite materials are outstanding due to high density and good mechanical properties. The product can be delivered both as semi-finished product for furthe.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 450 °C |
3.61 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck MoCu 85/15 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 6.50 - 7.90 µm/m-°C @Temperature 25.0 - 100 °C |
3.61 - 4.39 µin/in-°F @Temperature 77.0 - 212 °F |
|
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott K10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BALF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SK11 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 300 °C |
3.61 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SK5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.61 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott NG3 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 400 °C |
3.61 µin/in-°F @Temperature 68.0 - 752 °F |
|
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 200 °C |
3.61 µin/in-°F @Temperature 68.0 - 392 °F |
DIN EN 821-1 |
CeramTec Rubalit® IS 95 Alumina Rubalit® IS 95 is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at eleva.. |
|||
CTE, linear | 6.50 µm/m-°C @Temperature 20.0 - 200 °C |
3.61 µin/in-°F @Temperature 68.0 - 392 °F |
hardened to 62 HRC |
Bohler-Uddeholm O1 Cold Work Tool Steel Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha.. |