Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 399 °C |
7.40 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach Thermodur® 2365 EFS Extra Fine Structure - Hot Work Die Steel Description: Thermodur® 2365 is an Extra Fine Structure (EFS) hot work tool steel developed for good high temperature strength and tempering resistance and Supplied in the annealed conditionChara.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 649 °C |
7.40 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel CHRO-MOW® Tool Steel, AISI H12 Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 427 °C |
7.40 µin/in-°F @Temperature 70.0 - 800 °F |
|
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 538 °C |
7.40 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel LABELLE® Silicon #2 Tool Steel LaBelle Silicon #2 is a shock resisting tool steel capable of maximum toughness at relatively high hardness. It has excellent resistance to impact and battering, with good edge retention.Information.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 649 °C |
7.40 µin/in-°F @Temperature 70.0 - 1200 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
7.40 µin/in-°F @Temperature 70.0 - 200 °F |
|
Carlson C 600 Nickel-Chromium-Iron Alloy Carlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excellent resistance to c.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
7.40 µin/in-°F @Temperature 70.0 - 200 °F |
|
Carlson C 600ESR Nickel-Chromium-Iron Alloy General DescriptionCarlson Alloy C 600 is nickel-chromium alloy, developed for use in severely corrosive environments at elevated temperatures. The high nickel content of this alloy provides excell.. |
|||
CTE, linear | 13.3 µm/m-°C @Temperature 21.1 - 302 °C |
7.40 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach Formadur® 2311 Plastic Mold Steel Description: Formadur® 2311 is a pre-hardened plastic mold steelCharacteristics: Good texturing compared to Formadur®2312 and Good polishability compared to Formadur® 231Applications: Injection m.. |