Polymer Property : CTE, linear = 7.211 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 12.98 µm/m-°C

@Temperature 21.0 - 538 °C
7.211 µin/in-°F

@Temperature 69.8 - 1000 °F
Latrobe CM-50â„¢ ASTM M50 High Speed Steel
CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to..