Material Notes:
CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking tools, where toughness is of prime importance and where there is less need for red hardness.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.84 g/cc
7.84 g/cc
Density 7.83 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64
64
Oil Quenched from 1149°C
64.5
64.5
Oil Quenched from 1038°C
65
65
Oil Quenched from 1107°C
Modulus of Elasticity 203 GPa
29500 ksi
Machinability 65 - 75 %
65 - 75 %
1% Carbon Steel
Izod Impact Unnotched 36.6 J
27.0 ft-lb
Oil Quenched at 1121°C; 482°C Temper Temperature
67.8 J
50.0 ft-lb
Oil Quenched at 1121°C; 594°C Temper Temperature
74.6 J
55.0 ft-lb
Oil Quenched at 1121°C; 622°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 11.3 µm/m-°C

@Temperature 21.0 - 204 °C
6.28 µin/in-°F

@Temperature 69.8 - 399 °F
12.98 µm/m-°C

@Temperature 21.0 - 538 °C
7.211 µin/in-°F

@Temperature 69.8 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.84 %
0.84 %
Chromium, Cr 4.1 %
4.1 %
Iron, Fe 89.01 %
89.01 %
Manganese, Mn 0.30 %
0.30 %
Molybdenum, Mo 4.25 %
4.25 %
Silicon, Si 0.50 %
0.50 %
Vanadium, V 1.0 %
1.0 %
Chemical Properties Metric English Comments
Critical Temperature 730 °C
1350 °F
Ar1
751 °C
1380 °F
Ar3
810 °C
1490 °F
Ac1
846 °C
1550 °F
Ac3