Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.98 µm/m-°C @Temperature 21.0 - 538 °C |
7.211 µin/in-°F @Temperature 69.8 - 1000 °F |
|
Latrobe CM-50â„¢ ASTM M50 High Speed Steel CM-50 is classified as an intermediate type high speed steel of the molybdenum chromium- vanadium variety. It is recommended for applications with moderate cutting conditions, such as woodworking to.. |