Polymer Property : CTE, linear = 69.11 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 124.4 µm/m-°C

@Temperature 50.0 - 100 °C
69.11 µin/in-°F

@Temperature 122 - 212 °F
ASTM E831-00
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur..