Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 124.4 µm/m-°C @Temperature 50.0 - 100 °C |
69.11 µin/in-°F @Temperature 122 - 212 °F |
ASTM E831-00 |
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur.. |