Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.1 µm/m-°C @Temperature 600 °C |
6.72 µin/in-°F @Temperature 1110 °F |
|
Outokumpu 4742 High Temperature Ferritic Stainless Steel Good scaling resistance and can be subjected to reducing sulphur environments without risk. Subject to 475°C embrittlement and grain coarsening at temperatures above 950°C. s-phase may form afte.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 500 °C |
6.72 µin/in-°F @Temperature 68.0 - 932 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 500 °C |
6.72 µin/in-°F @Temperature 68.0 - 932 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 0.000 - 200 °C |
6.72 µin/in-°F @Temperature 32.0 - 392 °F |
|
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 500 °C |
6.72 µin/in-°F @Temperature 68.0 - 932 °F |
|
International Mold Steel DH31-EX Die Cast & Forging Steel DH31-EX is a hot working die steel with the best balance of strength and toughness showing the comparable softening resistance to SKD7 and twice hardenability as that of SKD61.Information provided b.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 649 °C |
6.72 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 1.5" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 200 °C |
6.72 µin/in-°F @Temperature 77.0 - 392 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Sheet, Solution Annealed and Cold Worked Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and la.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 2.25" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 3" RD High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 8" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800Â.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 40.0 - 540 °C |
6.72 µin/in-°F @Temperature 104 - 1000 °F |
|
Crucible Steel CPM® Rex M4 HC(HS) Tool Steel CPM REX M4 HC(HS) is a high vanadium special purpose high speed steel exhibiting better wear resistance and toughness than M2 or M3 in cold work punches, die inserts and cutting applications involvi.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 540 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel CPM® Rex® 54® (HS) High Speed Steel CPM Rex 54 is a cobalt-bearing high speed steel designed to offer an improvement in the red hardness of the popular M4 grade, while maintaining wear properties equivalent to M4. CPM Rex 54 has a che.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 540 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.72 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2 REX M2S (1.0C) is a sulfur-bearing high carbon version of the regular CRUCIBLE REX M2 high speed steel. The sulfur addition provides good grindability and an improvement in machinability of 25 to 35.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 21.1 - 538 °C |
6.72 µin/in-°F @Temperature 70.0 - 1000 °F |
|
Crucible Steel REX® M2 S High Speed Steel REX M2 is a tungsten-molybdenum high speed steel which gives outstanding performance in all operations where a general purpose high speed steel is required. REX M2 has a wide hardening range, excell.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 600 °C |
6.72 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature <=649 °C |
6.72 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature <=649 °C |
6.72 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature <=649 °C |
6.72 µin/in-°F @Temperature <=1200 °F |
|
AK Steel 420LC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 400 °C |
6.72 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels ASP 23 Cold Work Steel ASP 23 is a chromium-molybdenum-tungsten-vanadium alloyed high speed steel which is characterized by:High wear resistance (abrasive profile)High compressive strengthVery good through-hardening prope.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 100 °C |
6.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Alloy 255 Stainless Steel, UNS S32550 Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applicatio.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 350 °C |
6.72 µin/in-°F @Temperature 68.0 - 662 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 25.0 - 100 °C |
6.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |
|||
CTE, linear | 12.1 µm/m-°C @Temperature 20.0 - 538 °C |
6.72 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe Lescalloy® Jethete M-152 ESR 6" RCS High Strength Stainless Steel LESCALLOY JETHETE M-152 ESR is a nitrogen bearing, hardenable 12% chromium stainless steel intended for various structural components requiring high strength and good oxidation resistance up to 800°.. |