Material Notes:
Alloy 255 is a 25% chromium duplex ferritic-austenitic stainless steel designed to provide a superior combination of high strength and excellent corrosion resistance for a wide variety of applications. The alloy possesses a microstructure which is a balanced mixture of austenite and ferrite. The combination of these phases develops the unique combination of strength and chloride stress-corrosion cracking resistance of this alloy. The alloy finds applications in marine corrosion areas, equipment for phosphoric acid and fertilizer industry, pollutions control equipment, the pulp and paper industry and the petrochemical industry.Information provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 7.728 g/cc
0.2792 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 302
<= 302
Hardness, Rockwell C <= 32
<= 32
Tensile Strength, Ultimate >= 758 MPa
>= 110000 psi
Tensile Strength, Yield >= 552 MPa

@Strain 0.200 %
>= 80100 psi

@Strain 0.200 %
Elongation at Break >= 15 %
>= 15 %
in 2"
Charpy Impact 191 - 212 J
141 - 156 ft-lb
Thermal Properties Metric English Comments
CTE, linear 12.1 µm/m-°C

@Temperature 20.0 - 100 °C
6.72 µin/in-°F

@Temperature 68.0 - 212 °F
12.9 µm/m-°C

@Temperature 23.0 - 250 °C
7.17 µin/in-°F

@Temperature 73.4 - 482 °F
13.8 µm/m-°C

@Temperature 23.0 - 500 °C
7.67 µin/in-°F

@Temperature 73.4 - 932 °F
Specific Heat Capacity 0.481 J/g-°C

@Temperature 52.0 °C
0.115 BTU/lb-°F

@Temperature 126 °F
Component Elements Properties Metric English Comments
Carbon, C 0.040 %
0.040 %
Chromium, Cr 24 - 27 %
24 - 27 %
Copper, Cu 1.5 - 2.5 %
1.5 - 2.5 %
Iron, Fe 57 - 64 %
57 - 64 %
as balance
Manganese, Mn 1.5 %
1.5 %
Molybdenum, Mo 2.9 - 3.9 %
2.9 - 3.9 %
Nickel, Ni 4.5 - 6.5 %
4.5 - 6.5 %
Nitrogen, N 0.10 - 0.25 %
0.10 - 0.25 %
Phosphorous, P 0.040 %
0.040 %
Silicon, Si 1.0 %
1.0 %
Sulfur, S 0.030 %
0.030 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000821 ohm-cm
0.0000821 ohm-cm